Water spray is necessary when grinding on a zirconia ceramic coping. 

The white light or hot spot you see between a diamond and a zirconia ceramic has been measured at 1500 ºC. 

If the temperature of zirconia ceramic rises above 1000 ºC, a phase change can occur that will induce cracking and surface defects, lowering the strength of the coping.